Can't post a photo yet, but my piece titled "At The Lake" is done. It's 11:29 and went to about 1500degrees. The idea was to heat it just enough to keep it solid but not enough to loose the wonderful texture. I opened the kiln lid just long enough to let the heat out so it doesn't keep softening before it cools.
Can't wait till I can check it out. That is the hardest thing about any fusing process... having the patience to not open the kiln too soon.